ASTM C1097-06a Standard Specification for Hydrated Lime for Use in Asphalt Cement or Bituminous Pavements

standard by ASTM International, 11/15/2006

More details

In stock

$22.36

-57%

$52.00

More info

Full Description

1.1 This specification covers high calcium, dolomitic and magnesian-hydrated lime for use in asphalt cement or bituminous pavement.

Note 1

Hydrated lime, either calcitic, dolomitic, or magnesian, improves bonding of bitumen and aggregates which reduces susceptibility to moisture damage, reduces age hardening by chemically stabilizing polar compounds found in asphalts, and increases initial stiffness of asphalt mixtures.

Note 2

No attempt is made to present requirements for any by-product lime.